A diamond, ceramic, metal, or metal alloy surface is coated with molten CrO3. The coated surface is then heated in air at a temperature of from about 200 DEG C. to 250 DEG C. until the molten CrO3 coating is converted into a black, powdery adherent coating of CrO.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for forming CrO coatings comprising: A. coating a diamond, ceramic, metal, or metal alloy surface with molten CrO 3 ; and B. heating the molten CrO 3 coated surface formed in step A in air at a temperature of from the melting point of CrO 3 up to 250° C. until the CrO 3 is converted into CrO in the form of an adherent, powdery, black coating.

  2. Claim 2Depends on #1

    The process of claim 1 wherein the molten CrO 3 coated surface is heated in step B at a temperature of from 200° C. to 240° C.

  3. Claim 3Depends on #2

    The process of claim 2 wherein the molten CrO 3 coated surface is heated in step B at a temperature of from 210° C. to 230° C.