Process for manufacturing an oxidation-stable component on a CFC base, particularly for space travel
Abstract
For the manufacturing of an oxidation-stable component that can withstand temperature changes for space travel, a solid CFC-body with a density of from 0.1 to 0.8 g/cm 3 , which has nondirectional short fibers, is made from short carbon fibers and a hardenable resin binder. From the solid CFC-body, a CFC-blank having the dimensions of the component to be manufactured is prepared by means of turning or other material cutting. The CFC-blank is infiltrated with pyrolytic carbon to a density of no more than 1.0 g/cm 3 and then with metallic silicon so that its density amounts to more than 2.0 g/cm 3 . A portion of the metallic silicon is reacted with the pyrolytic carbon to form silicon carbide. The proportion of the unreacted metallic silicon which remains in the component after this reaction amounts to at least 15 percent by weight.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 24.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for manufacturing an oxidation stable component for use in space travel and in temperature environment of at least 1500° C. from a solid CFC-body, comprising the steps of: preparing a solid CFC-body with a density of from 0.1 to 0.6 g/cm 3 from short carbon fibers in an amount of from 5 to 60 percent by weight suspension in a hardenable resin binder, by filling the suspension into a mold corresponding to a shape of the solid CFC-body, removing the solvent from the suspension, and thermosetting and carbonizing the resin binder; machining said solid CFC-body to a desired shape and d
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗