Comprehensive process for low temperature epitaxial growth
Abstract
A system and method for growing low defect density epitaxial layers of Si on imperfectly cleaned Si surfaces by either selective or blanket deposition at low temperatures using the APCVD process wherein a first thin, e.g., 10 nm, layer of Si is grown on the surface from silane or disilane, followed by the growing of the remainder of the film from dichlorosilane (DCS) at the same low temperature, e.g., 550° C. to 850° C. The subsequent growth of the second layer with DCS over the first layer, especially if carried out immediately in the very same deposition system, will not introduce additional defects and may be coupled with high and controlled n-type doping which is not available in a silane-based system. Further, in order to achieve an optimal trade-off between the need for an inert ambience to promote silane reaction at low temperature and the need for a hydrogen ambience to prevent surface oxidation from inadvertant residual impurities, depositions are carried out in an ambience composed primarily of He but always containing some H 2 . Also, the relative deposition rates on a patterned surface of polycrystalline Si on insulator areas and single crystal Si on single crystal seed
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 39.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for minimizing defect density in growing epitaxial films of Si by deposition at low temperatures on a receiving surface at low or atmospheric pressure, comprising the steps of: providing an ambience of gas for said receiving surface composed of hydrogen, a silane, and an inert gas comprising from about 20% to about 95% of the total gas; first growing a layer of Si from said silane on said receiving surface, at a temperature in the range from about 550 degrees C. to about 850 degrees C.; and followed by the growing of the remainder of the Si film from dichlorosilane at a low temper
- Claim 2Depends on #1
A method as in claim 1 wherein said growing from silane is continued until the growth is in the form of blanket deposition.
- Claim 3Depends on #1
A method as in claim 1 wherein said temp
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗