US 5,376,601 A#3832963 Most CitedExpiredUnited States (USPTO)Utility

Sintered product of aluminum nitride, a process for the preparation thereof, and a baking jig using the same

21Forward Citations (#3832963 Global)
0.7/yrCitation Velocity (#12136468 Global)
5.69Citation PageRank (#2687611 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A molded article is prepared from an AlN powder of a high purity without adding sintering assistant, baked in a nitrogen atmosphere without containing carbon, and is further heat-treated in a nitrogen atmosphere containing carbon in order to remove impurities in the sintered product. There is obtained a highly pure and dense sintered product which comprises mainly a phase of aluminum nitride, which has an average grain size of greater than 9 μm, cationic metal impurities other aluminum, and Si, Fe and Ca in amounts smaller than predetermined values. The sintered product exhibits a very small creep rate when stress is applied thereto at high temperatures and is used as a material for high temperature uses such as a baking jig. Owing to its excellent anti-creeping property at high temperatures, tile product is suitably used as a structural material subject to stress at high temperatures for extended periods of time. When used as a baking jig, in particular, the sintered product does not adversely affect the molded articles and exhibits excellent durability.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 21.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A sintered product of aluminum nitride which has been sintered without addition of a sintering assistant, consisting essentially of a single phase of aluminum nitride, having an average grain size of greater than 9 μm, cationic metal impurities other than aluminum in a total amount smaller than 0.3% by weight, Si in an amount smaller than 1000 ppm, Fe in an amount smaller than 150 ppm, and Ca in an amount smaller than 200 ppm, and carbon in an amount smaller than 0.3% by weight, and having a relative density of greater than 90%, wherein when a transverse test piece prepared therefrom in compli

  2. Claim 2Depends on #1

    A sintered product of aluminum nitride according to claim 1, wherein the c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 21 total)

PatentTitleYearCitations
US 6,174,583 B1Aluminum nitride sintered body, metal including member, electrostatic chuck, method of producing aluminum nitride sintered body, and method of producing metal including member200123
US 2007142204 A1Crystalline composition, device, and associated method—14
US 6,475,924 B2Substrate and process for producing the same200216
EP 0,771,772 A3Aluminium nitride sintered bodies and their manufacture—0
US 6,084,221 AAluminum nitride heater200013
US 5,755,570 AApparatus for in situ environment sensitive sealing and/or product controlling199831
US 5,911,945 AMethod for in-situ environment sensitive sealing and/or product controlling19992
EP 0,798,278 A3Aluminium nitride sintered body, metal embedded article, electronic functional material and electrostatic chuck—0
KR 100,268,481 B1Aluminium nitride sintered body, metal embedded article, electronic functional material and electrostatic chunk20000
US 5,998,320 AAluminum nitride sintered body, metal including member, electrostatic chuck, method of producing aluminum nitride sintered body, and method of producing metal including member199919
EP 4,317,058 A4Aluminum nitride granular powder and resin composition—0
CN 109,576,783 AA kind of preprocessing method of raw materials for high quality aluminum nitride crystal growth—8
EP 1,128,425 A1Aluminium nitride sintered body, metal embedded article, electronic functional material and electrostatic chuck—2
US 5,911,102 AMethod of manufacturing sintered compact199959
US 6,027,686 AMethod of manufacturing sintered compact200045