Reinforced resin composition
Abstract
A reinforced resin composition comprising 100 parts by weight of a resin component comprising a polycarbonate resin, a thermoplastic polyester resin and an impact modifier in a ratio, by weight, of 90-10:10-90:0-40 and 0.5 to 100 parts by weight of kaolin with a mean particle diameter of 0.1 to 4.0 μm. The composition can be molded by conventional techniques such as injection molding and extrusion molding into automotive parts, electrical or electronic parts and other products excellent in heat resistance, impact resistance, rigidity, dimensional stability, chemical resistance, moldability, weather resistance and thermal stability with a low linear coefficient of expansion and excellent surface gloss and appearance.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 23.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A reinforced resin composition comprising 100 parts by weight of a resin component comprising a polycarbonate resin, a thermoplastic polyester resin and an impact modifier in a ratio, by weight, of 90-10:10-90:0-40 and 0.5 to 100 parts by weight of a kaolin with a mean particle diameter of 0.2 to 2.0 μm.
- Claim 2Depends on #1
A reinforced resin composition as claimed in claim 1 which comprises 100 parts by weight of a resin component comprising a polycarbonate resin, a thermoplastic polyester resin and an impact modifier in a ratio, by weight, of 90-10:10-90:1-20 and 0.5 to 100 parts by weight of a kaolin with a mean particle diameter of 0.2 to 2.0 μm.
- Claim 3Depends on #1
A reinforced resin composition as claimed in claim 1 wherein said polycarbonate resin has a viscosity average molecular weight of 10,000 to 60,000.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗