Patents
US 5,364,720 A#2885117 Most CitedExpiredUnited States (USPTO)Utility

Magnetic developer for developing electrostatic images

26Forward Citations (#2885117 Global)
0.8/yrCitation Velocity (#9054719 Global)
3.32Citation PageRank (#6421237 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A magnetic developer for developing electrostatic images is constituted by magnetic toner particles, each containing a binder resin having a melt viscosity of at most 5.0×10 6 poise at 150° C. and a magnetic material. The magnetic material is blended with a proportion (C) [wt. %] of inorganic fine particles based on the magnetic material to carry 0.2-5 wt. % of the inorganic fine particles secured to the magnetic material surface. The magnetic material has a specific surface area (A) [m 2 /g] before securing of the inorganic fine particles and is provided with an increase in surface area (B) [m 2 /g] by the securing of the inorganic fine particles; wherein the parameters A, B and C satisfy the following formulae (1) and (2): 0.1≦B/A≦0.8 (1) B<30×C (2). As a result, the magnetic developer is provided with an improved low-temperature fixability without causing problems accompanying the use of a low-temperature softening binder resin, such as deterioration of anti-offset characteristic, storage characteristic, developing characteristic.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 26.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A magnetic developer for developing electrostatic images, comprising: magnetic toner particles, each containing a binder resin having a melt viscosity of at most 5.0×10 6 poise at 150° C. and a magnetic material, wherein said magnetic material is blended with a proportion (C) [wt. %] of inorganic fine particles based on the magnetic material to carry 0.2-5 wt. % of the inorganic fine particles secured to the magnetic material surface, and said magnetic material has a specific surface area (A) [m 2 /g] before securing of the inorganic fine particles and is provided with an increase in surfa

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗