Acid treatment of poly(arylene sulfide) polymer reaction mixture
Abstract
A method is provided for producing a poly(arylene sulfide) polymer having reduced amounts of impurities by contacting a poly(arylene sulfide) polymerization reaction mixture with an acid.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 8.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for producing a poly(arylene sulfide) polymer which comprises contacting reactants comprising at least one sulfur source, at least one dihaloaromatic compound and a polar organic compound to form a polymerization reaction mixture, subjecting said polymerization reaction mixture to suitable polymerization conditions to form said poly(arylene sulfide) polymer, contacting said reaction mixture with an acidic solution while maintaining said suitable polymerization conditions, and thereafter recovering said poly(arylene sulfide) polymer.
- Claim 2Depends on #1
A process according to claim 1 wherein said suitable conditions comprise a polymerization reaction temperature in the range of about 235° to about 450° C.
- Claim 3Depends on #1
A process in accordance with claim 1 wherein the amount of acidic solution employed is in the range
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (9)
Non-Patent Literature (4)
- Derwent Abstract Japanese application Publication No. JP 62 205125.
- Derwent Abstract Japanese application Publication No. JP 62 223232.
- Derwent Abstract Japanese application Publication No. JP 62-205125.
- Derwent Abstract Japanese application Publication No. JP 62-223232.