Process for etching high copper content aluminum films
Abstract
Aluminum alloys containing high amounts of copper can be etched to eliminate copper residues using boron trichloride and chlorine under etch conditions of low temperature, low pressure, high power and strict control of the amount of nitrogen present.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 33.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for reactive ion etching of an aluminum alloy containing over about 0.5% of copper on a substrate which comprises etching with a precursor gas including boron trichloride and chlorine at temperatures below about 80° C. while regulating the nitrogen content of the precursor gases to prevent formation of a copper residue on the substrate.
- Claim 2Depends on #1
A method according to claim 1 wherein the temperature is maintained at about 60°-65° C. during etching.
- Claim 3Depends on #1
A method according to claim 1 wherein said aluminum alloy has a layer selected from the group consisting of TiN, TiW and W thereover or thereunder.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 33 total)
References Cited — Backward Prior Art (4)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,370,196 A | Anisotropic etching of aluminum | 1983 | 14 |
| US 4,798,650 A | Method of dry etching aluminum | 1989 | 38 |
| US 4,951,601 A | Multi-chamber integrated process system | 1990 | 968 |
| US 4,985,113 A | Sample treating method and apparatus | 1991 | 48 |