Patents
US 5,348,618 A#280159 Most CitedExpiredUnited States (USPTO)Utility

Method of making silicon quantum wires

92Forward Citations (#280159 Global)
2.9/yrCitation Velocity (#974748 Global)
24.05Citation PageRank (#245338 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of making semiconductor quantum wires employs a semiconductor wafer as starting material. The wafer is weakly doped p type with a shallow heavily doped p layer therein for current flow uniformity purposes. The wafer is anodised in 20% aqueous hydrofluoric acid to produce a layer microns thick with 70% porosity and good crystallinity. The layer is subsequently etched in concentrated hydrofluoric acid, which provides a slow etch rate. The etch increases porosity to a level in the region of 80% or above. At such a level, pores overlap and isolated quantum wires are expected to form with diameters less than or equal to 3 nm. The etched layer exhibits photoluminescence emission at photon energies well above the silicon bandgap (1.1 eV) and extending into the red region (1.6-2.0 eV) of the visible spectrum.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 92.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing silicon quantum wires comprising the steps of: (1) anodizing crystalline silicon material (14) to produce a porous layer therein, and (2) etching the porous layer to widen the pores sufficiently to produce pore overlap thereby defining discrete quantum wires.

  2. Claim 2Depends on #1

    A method according to claim 1 wherein said etching step includes etching to form discrete quantum wires with a width not greater than 3 nm.

  3. Claim 3Depends on #1

    A method according to claim 1 wherein said anodizing step produces porosity in the range 20% to 80%, and said etching step includes etching at a rate in the range 0.0001 nm to 10 nm per minute to provide an increase in porosity to a value in the range 60% to 90%.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Applied Physics Letters, vol. 57, No. 10, Sep. 3, 1990, New York, pp. 1046 2048, L. T. Canham, Silicon Quantum Wire Array Fabricatin By Electrochemical and Chemical Dissolution of Wafers .
  • Applied Physics Letters, vol. 57, No. 10, Sep. 3, 1990, New York, pp. 1046-2048, L. T. Canham, "Silicon Quantum Wire Array Fabricatin By Electrochemical and Chemical Dissolution of Wafers".
  • Journal of Vacuum Science and Technology: Part B., vol. 4, No. 1, 1986, New York, pp. 365 368; A. C. Warren et al., Fabrication Of Sub 100NM Linewith Periodic Structures For Study of Quantum Effects From Interference and Confinement in SI Inversion Layers .
  • Journal of Vacuum Science and Technology: Part B., vol. 4, No. 1, 1986, New York, pp. 365-368; A. C. Warren et al., "Fabrication Of Sub-100NM Linewith Periodic Structures For Study of Quantum Effects From Interference and Confinement in SI Inversion Layers".
  • Leveling Using Radiotracer Techniques, vol. 107, No. 9, "Electrochemiluminescence at a Silicon Anode in Contact with an Electrolyte", pp. 787-788, Sep. 1960.