A copolymer of maleic anhydride and an alkyl vinyl ether is stabilized by contacting same with a non-reactive substantially moisture free gas at a temperature of from about 30°-100° C. for from about 0.5-24 hours. The copolymer is preferably prepared by reacting together maleic anhydride and an alkyl vinyl ether in the presence of a free radical initiator.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of copolymers of maleic anhydride and alkyl vinyl ethers having a stable specific viscosity, which comprises: providing a copolymer of maleic anhydride and an alkyl vinyl ether, wherein the alkyl group contains from 1 to 5 carbon atoms; contacting said copolymer with a flowing stream of non-reactive substantially moisture free gas at a temperature of from about 30°-100° C. for from about 0.5-24 hours at sub-critical pressure, thereby stabilizing the specific viscosity of the copolymer and providing a copolymer which does not degrade on storage or upon exposure to

  2. Claim 2Depends on #1

    Process according to claim 1 wherein the gas is nitrogen.

  3. Claim 3Depends on #1

    Process according to claim 1 wherein the temperature is from about 40°-85° C.