Patents
US 5,334,341 A#12231466 Most CitedExpiredUnited States (USPTO)Utility

Process for controlling carbon content of injection molding steels during debinding

9Forward Citations (#12231466 Global)
0.3/yrCitation Velocity (#27187967 Global)
1.50Citation PageRank (#22776247 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for controlling the carbon content in a metallic piece molded by injection or other process comprising, a) heating the shaped piece under a 100% hydrogen atmosphere up to about 200° C., b) replacing the 100% H 2 atmosphere by a substantially 100% nitrogen atmosphere and heating the pieces from 200° C. to 450° C., c) maintaining the temperature in the enclosure at substantially 450° C. while subjecting the pieces to an atmosphere comprising from 15% to 100% vol. hydrogen, the complement being nitrogen, then d) replacing the atmosphere by a substantially 100% nitrogen and e) heating the pieces from 450° C. to substantially 700° C. in order to further eliminate the remaining binder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for controlling the carbon content in a metallic piece molded by injection or other process comprising, a) heating said shaped piece under a substantially pure hydrogen atmosphere only up to a temperature sufficient to remove low molecular weight constituents, b) replacing said substantially pure H 2 atmosphere with a substantially pure nitrogen atmosphere and heating the pieces to a temperature higher than that in step a), sufficient to remove binder without effecting carburization or decarburization, c) maintaining the temperature in the enclosure at substantially the same tem

Technical Overview & Description