Abstract

A high-strength silicon nitride sintered body having a flexural strength of 100 kg/mm2 or higher and a process for producing the same are disclosed, the sintered body comprising not less than 90% by weight of a single crystalline phase of silicon aluminum oxynitride (Si6-zAl2OzN8-z, wherein z is a number of from 0 to 4.2) having an average longer diameter of not more than 5 mu m and an aspect ratio of not less than 5, the crystal phase constituting a network structure in the sintered body, the balance being a crystalline or amorphous (glassy) phase comprising one or more of oxides or oxynitrides of a rare earth metal, a group 3A metal, a group 2A metal or Si, and the process comprising mixing silicon nitride powder, an organic metal salt as a first sintering aid, and at least one of a metal oxide, a metal nitride, and a metal oxynitride as a second sintering aid, either separately or as a mixture of two or more thereof, with a solvent and a surface active agent, subjecting the mixture or mixtures to ultrasonic dispersion, mixing the mixtures together followed by drying to obtain a mixed powder, molding the mixed powder, and sintering the molded article at a temperature of from 1,60

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A high-strength silicon nitride sintered body having a flexural strength of 130 kg/mm 2 or higher and a Weibull modulus of 15 or more, which consists essentially of not less than 90% by weight of a single crystalline phase of silicon aluminum oxynitride of the formula Si 6-z Al 2 O z N 8-z , where z is a number of from 0 to 4.2, which silicon aluminum oxynitride comprises crystals having an average longer diameter of from 2 to 5 μm and an aspect ratio of from 5 to 10, said crystalline phase constituting a network structure in the sintered body, the balance being a crystalline or amorphous

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Chemical Abstracts, vol. 106, No. 4, Jan. 1987, abstract No. 22274b Journal of Materials Science, vol. 24, No. 5, May 1989, pp. 1853 1861.