Process for manufacturing cold-rolled steel sheets with high-strength, and high-ductility and its named article
Abstract
The primary object of the present invention is to provide a cold-rolled steel sheet with properties of high-strength, high-ductility, and a process for manufacturing it. The constituents of the cold-rolled steel sheet comprise: 0.08%-0.25% carbon by weight, 0.03%-2.0% silicon by weight, 0.6%-1.8% manganese by weight, 0.01%-0.10% niobium by weight, 0.01%-0.08% aluminium by weight, with the rest being substantially iron and unnoticed impurities. The process for manufacturing cold-rolled steel sheets of the present invention by using the molten steel material as described above includes the following steps: (a) preparing steel ingots by continuous casting the molten steel; (b) hot rolling the steel ingots into hot-rolled bands; (c) coiling the hot-rolled bands at a temperature below 600° C.; (d) after cold-rolling, forming steel sheets from the hot-rolled bands and soaking the steel sheets at a temperature in the two-phase range (equal to AC1+10° C.-AC3-10° C. shown in FIG. 1) for a time duration ranging from 1 minute to 10 minutes; (e) cooling the steel sheets to a temperature ranging from 350° C. to 500° C. at a cooling rate greater than 50° C./SEC; (f) soaking the steel sheets at a
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 58.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A cold-rolled steel sheet consisting essentially of: 0.08%-0.25% carbon by weight, 0.3%-2.0% silicon by weight, 0.6%-1.8% manganese by weight, 0.01%-0.10% niobium by weight, 0.01%-0.08% aluminium by weight, substantial iron, and unnoticed impurities and having a microstructure with at least 8% retained austenite by volume fraction.
- Claim 2Depends on #1
A process for manufacturing cold-rolled steel sheets with properties of high-strength and high-ductility, by using the molten steel material as recited in claim 1, comprising the following steps: (a) preparing steel ingots by continuous casting the molten steel; (b) hot rolling the steel ingots into hot-rolled bands; (c) coiling the hot-rolled bands at a temperature below 600° C.; (d) after cold-rolling, forming steel sheets from the hotrolled bands and soaking the steel sheets at a temperature
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 58 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| JP S555584 A | Telephone set | — | 2 |
| JP S56127732 A | Preparation of high tensile cold rolling steel plate | — | 3 |