Thermoplastic polyester with reduced flammability
Abstract
Disclosed is a thermoplastic polyester with reduced flammability obtained by: (a) condensating an aromatic dicarboxylic acid and an alkylene glycol in a mole ratio of from 1:1.1-1.5 at a temperature of from 180° to 240° C. in the presence of a catalyst; (b) adding a polyalkylene glycol phosphate ester; (c) polycondensating at a temperature of from 265° to 280° C. under a pressure decreasing from 760 torr to less than 2 torr until an intrinsic viscosity of about 0.5 to about 0.7 is reached.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 12.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A thermoplastic polyester obtained by: (a) condensating an aromatic dicarboxylic acid or a lower alkyl ester thereof and an alkylene glycol in a mole ratio of from 1:1.1-1.5 at a temperature of from 180°0 to 240° C. in the presence of a catalyst; (b) adding a polyalkylene glycol phosphate ester of the general formula: ##STR2## wherein n is a number of from 1 to 10 m is a number of from 0 to 3; (c) polycondensating at a temperature of from 265° to 300° C. under a pressure decreasing from 760 torr to less than 2 torr until an intrinsic viscosity of about 0.5 to about 0.7 is reached.
- Claim 2Independent Claim
The polyester according to claim wherein the aromatic dicarboxylic acid is selected from the group consisting of terephthalic acid, isophthalic acid, 5-sulfo-isophthalic acid, diphenyl-para, para -dicarboxylic acid, para-phenylenediacetic acid, 2, 5-, 2
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,298,709 A | Polyhydroxyl polyether compounds containing phosphorus and polymeric resins prepared therefrom | 1981 | 29 |
| US 5,132,391 A | Polyester compositions | 1992 | 12 |