Patents
US 5,308,596 A#987107 Most CitedExpiredUnited States (USPTO)Utility

Process for the production of crystalline sodium disilicate in an externally heated rotary kiln having temperature zones

49Forward Citations (#987107 Global)
1.5/yrCitation Velocity (#3363044 Global)
3.48Citation PageRank (#5961282 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

To prepare crystalline sodium disilicates having a laminar structure, a molar ratio of SiO 2 to Na 2 O of (1.9 to 2.1) 1 and a water content of less than 0.3% by weight, a water glass solution is first obtained by reacting sand with sodium hydroxide solution in a molar ratio of SiO 2 to Na 2 O of (2.0 to 2.3) : 1 at temperatures of 180° to 240° C. and pressures of 10 to 30 bar. This water glass solution having at least 20% by weight of solids is treated in a spray drier with hot air at 200° to 300° C. with the formation of a pulverulent amorphous sodium disilicate having a water content (determined as loss on heating at 700° C.) of 15 to 23% by weight and a bulk density of at least 300 g/l. The spray-dried pulverulent, amorphous sodium disilicate is ground. The ground sodium disilicate is introduced into a rotary kiln equipped with devices for moving solids, externally heated via the wall and having in its interior a plurality of different temperature zones, and is treated therein at temperatures of 400° to 800° C. for 1 to 60 minutes with formation of crystalline sodium disilicate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 49.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of crystalline sodium disilicates having a laminar structure, a molar ratio of SiO 2 to Na 2 O of (1.9 to 2.1) : 1 and a water content of less than 0.3% by weight, which comprises: reacting sand with sodium hydroxide solution in a molar ratio of SiO 2 to Na 2 O of (2.0 to 2.3): 1 at temperature of 180° to 240° C. and pressures of 10 to 30 bar with formation of a water glass solution having at least 20% by weight of solids; spray-drying the water glass solution with hot air at 200° to 300° C. with the formation of a pulverulent amorphous sodium disilicate havin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Perry s Chemical Engineers Handbook (6th Ed.), Green & Maloney (ed), 1984, pp. 20 29 to 29 38.
  • Perry's Chemical Engineers' Handbook (6th Ed.), Green & Maloney (ed), 1984, pp. 20-29 to 29-38.