US 5,307,201 A#3357047 Most CitedExpiredUnited States (USPTO)Utility

Electrode of nickel oxide intercalated with lithium ions and electrochromic devices which incorporate such an electrode

23Forward Citations (#3357047 Global)
0.7/yrCitation Velocity (#10517327 Global)
6.05Citation PageRank (#2427476 Global)
2Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An electrode of nickel oxide intercalated with lithium ions, is obtained by: thermally evaporating, under vacuum, nickel oxide (Ni 2 O 3 ) and depositing on a conductive glass substrate a film of nickel oxide in which the atomic ratio of nickel to oxygen is comprised within the range of from 0.7:1 to 0.9:1, up to a thickness of the order of 100 nm; and activating the thin film of nickel oxide by electrochemical intercalation of an amount of lithium ions, which corresponds to a charge level of from 100 to 1,000 C/m 2 . An electrochromic window is disclosed, which comprises: (a) an electrode of tungsten oxide (WO 3 ) on a transparent, conductive glass sheet; and (b) an electrode of nickel oxide activated by electrochemical intercalation of lithium metal, on a transparent, conductive glass sheet; (c) an electrolyte interposed between the (a) electrode and the (b) electrode; wherein the nickel oxide electrode was obtained as said hereinabove.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 23.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An electrode of nickel oxide intercalated with lithium ions, which is prepared by steps of: (a) depositing on a conductive glass substrate a thin film of nickel oxide having a nickel to oxygen atomic ratio of from 0.7:1 to 0.9:1 and a thickness of up to 100 nm, the deposition being carried out by thermally evaporating nickel oxide (Ni 2 O 3 ); and (b) activating said thin film of nickel oxide by electrochemical intercalation of an amount of lithium ions which corresponds to a charge level of from 100 to 1,000 C/m 2 .

  2. Claim 2Depends on #1

    An electrode according to claim 1 wherein the depositing step is carried out under a vacuum of approximately 10- 4 Pa, at a temperature of about 2,000° C., and with a peposition rate of the order of 0.1 nm/second.

  3. Claim 3Depends on #1

    An electrode according to claim 1, wherein the activation by intercalation with lithiu

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 23 total)

PatentTitleYearCitations
US 2007097481 A1Electrochromic devices having improved ion conducting layers—101
US 8,004,744 B2Electrochromic devices having improved ion conducting layers201119
US 7,564,611 B2Electrode comprising lithium nickel oxide layer, method for preparing the same, and electrochromic device comprising the same200917
US 6,246,508 B1High voltage electrochromic device200110
US 6,061,168 AAll-solid electrochromic anti-glare mirror20003
US 2010014145 A1Electrode comprising lithium nickel oxide layer, method for preparing the same, and electrochromic device comprising the same—9
US 8,057,713 B2Method for the production of nickel oxide surfaces having increase conductivity20110
US 2008280204 A1Method For The Production Of Nickel Oxide Surfaces Having Increase Conductivity—1
CN 112,285,981 BPreparation method of electrochromic device with high charge storage capacity20220
KR 100,957,686 B1Electrode comprising lithium nickel oxide layer, method for preparing the same, and electrochromic device comprising the same20100
US 7,999,991 B2Electrode comprising lithium nickel oxide layer, method for preparing the same, and electrochromic device comprising the same20110
CN 115,259,245 AQuantitative lithiated nickel oxide electrochromic film and preparation method thereof—1
US 8,730,552 B2Electrochromic devices having improved ion conducting layers20143
WO 2007/081121 A1Electrode comprising lithium nickel oxide layer, method for preparing the same, and electrochromic device comprising the same—3
WO 9,807,067 A1High voltage electrochromic devices, the method of preparation thereof and the use of a specific non-aqueous electrolyte in electrochromic devices—0

Non-Patent Literature (5)

  • Canon, Patent Abstracts of Japan Production of Total Solid State Electrochromic Element, Oct. 12, 1984; and JP A 59 105618, Jun. 19, 1984.
  • Canon, Patent Abstracts of Japan-Production of Total Solid State Electrochromic Element, Oct. 12, 1984; and JP-A-59-105618, Jun. 19, 1984.
  • Patent Abstracts of Japan Manufacture of Electrode for Solid Electrolyte Type Fuel Cell, vol. 14, No. 273, Jun. 13, 1990, and JP A 2 087 470 (Mar. 28, 1990).
  • Patent Abstracts of Japan-Manufacture of Electrode for Solid Electrolyte Type Fuel Cell, vol. 14, No. 273, Jun. 13, 1990, and JP-A-2 087 470 (Mar. 28, 1990).
  • S. Passerini et al. The Intercalation of Lithium in Nickel Oxide and its Electrochromic Properties Journal of the Electrochemical Society, vol. 137, Oct. 10, 1990, pp. 3297 3300.