Patents
US 5,294,398 A#61518099 Most CitedExpiredUnited States (USPTO)Utility

Low temperature heat shrinkable film and process for producing the same

1Forward Citations (#61518099 Global)
0.0/yrCitation Velocity (#59023381 Global)
0.75Citation PageRank (#61518099 Global)
10Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a low temperature heat shrinkable film comprising a linear low density polyethylene resin having a short branched chain and a density of 0.935 g/cm 3 , and whose film properties are such that the haze value is 5% or less, the heat shrinkages at 90° C. in the M and T directions are 30% or more and 5% or less, respectively , and the shrinkage stress at 90° C. in the M direction is 300 g/mm 2 or more. This transparent film having an excellent low temperature heat shrinkability can be produced by drawing a film of the above-mentioned polyethylene resin between two rolls having a diameter of 200 mm or less at an air gap of 10 mm or less at a draw ratio of 3.0 to 6.0. Further, an inflation film having a multilayer structure can be obtained by press bonding or press bonding and drawing a plurality of films comprising the above-mentioned polyethylene resin. This laminate film has an excellent transparency and strength, and has a uniform film thickness.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for producing a low temperature heat shrinkage film, comprising: drawing a linear low density polyethylene resin film having a short branched chain and a density of 0.935 g/cm 3 or less between two rolls having a diameter of 200 nm or less at an air gap of 10 mm or less at a draw ratio of 3.0 to 6.0.

  2. Claim 2Depends on #1

    A process according to claim 1, wherein the linear low density polyethylene resin has a density of 0.900 to 0.935 g/cm 3 .

  3. Claim 3Depends on #1

    A process according to claim 1, wherein the linear low density polyethylene resin has a melt index of 0.3 to 8 g/10 min.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)