Presulfurized hydrotreating, hydrocracking or tail gas treating catalyst

10Forward Citations (#10147862 Global)
0.3/yrCitation Velocity (#25041088 Global)
2.50Citation PageRank (#10149330 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention relates to an unproved method of presulfurizing a sulfidable metal oxide(s)-containing catalyst which minimizes sulfur stripping upon start-up of a reactor and improves catalyst activity. The method consists of contacting a sulfidable metal oxide(s)-containing catalyst with elemental sulfur at a temperature such that said elemental sulfur is substantially incorporated in the pores of said catalyst by sublimation and/or melting and heating the sulfur-incorporated catalyst in the presence of a liquid olefinic hydrocarbon at a temperature greater than about 150° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 10.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A presulfurized catalyst composition prepared by a process which comprises: (a) contacting a presulfidable metal oxide(s)-containing catalyst with elemental sulfur at a temperature such that said elemental sulfur is substantially incorporated in the pores of said catalyst by sublimation and/or melting and (b) heating said sulfur-incorporated catalyst in the presence of a liquid olefinic hydrocarbon at a temperature greater than about 150° C.

  2. Claim 2Depends on #1

    The composition of claim 1 wherein the temperature in step (b) ranges from about 150° C. to about 350° C.

  3. Claim 3Depends on #2

    The composition of claim 2 wherein the temperature ranges from about 200° C. to about 325° C.