Patents
US 5,290,508 A#9223581 Most CitedExpiredUnited States (USPTO)Utility

Manufacturing process for ring-shaped parts

11Forward Citations (#9223581 Global)
0.3/yrCitation Velocity (#22529784 Global)
2.39Citation PageRank (#10892546 Global)
10Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a manufacturing process for ring-shaped parts having high wear resistance and mechanical strength. Raw material powder containing (weight %) C at 0.4-0.9%, Ni at 1.5-4.0%, Mo 0.2-0.6%, and a remainder consisting of Fe and unavoidable impurities, is compacted and shaped, thereafter sintered and forged; obtained sintered body is hardened by heating at a temperature within a range of 800°-950° C., thereafter high temperature tempering is carried out for 20-60 minutes at a temperature within a range of 570°-700° C.; then the surface layer of the inner periphery and/or outer periphery of said sintering body is heated; then if required, low temperature tempering (temper process) is carried out at a temperature within a range of 160°-220° C., and whereby the hardness of the surface layer, for which abrasive resistance is required, reaches a value of HRC 58-63 degree, and the hardness of the middle layer falls within a range of HRC 25-40 degree.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 11.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A manufacturing method for ring-shaped parts, characterized in that a raw material powder composition comprising C at 0.4-0.9% by weight, Ni at 1.5-4.0% by weight, Mo at 0.2-0.6% by weight, and a remainder consisting of Fe and unavoidable impurities, is compacted; thereafter sintered and forged; then, after obtained sintered body is heated at a temperature within a range of 800°-950° C., high temperature tempering is carried out for 20-60 minutes at a temperature within a range of 570°-700° C., then the surface layers of the inner periphery and/or the outer periphery of said sintered body is s

  2. Claim 2Depends on #1

    A manufacturing method for ring-shaped parts according to claim 1, characterized in that the hardening treatment of the surface layer of the sintered body is performed by heating within a range 800°-950° C.,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗