Method for producing regular grain oriented electrical steel using a single stage cold reduction
Abstract
The present invention produces a regular grain oriented electrical steel using a single cold reduction step having excellent and highly uniform magnetic quality. The method includes the steps of providing an electrical steel band having Mn of 0.024% or less in excess of that needed to combine with S and/or Se. The band is provided with an anneal at a temperature of from 900°-1125° C. (1650°-2050° F.) for a time up to 10 minutes and slowly cooled to 480°-650° C. (900°-1200° F.) followed by rapid cooling to a temperature below 100° C. (212° F.). The annealed band must have a critical amount of austenite, γ 1150 ° C., of 7% or more. The annealed band is cold reduced in a single stage to the desired final thickness. The strip is decarburized and provided with an annealing separator coating on one or more surfaces of the strip. Before or during the final high temperature anneal, a total S level at least 15 mg per square meter is provided. The strip is final annealed at a temperature of 1100° C. or higher to effect secondary grain growth. The finished regular grain oriented electrical steel has far superior and more uniform magnetic quality than available from previous single stage proce
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 17.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing regular grain oriented electrical steel having a permeability measured at 796 A/m of from 1780 to 1880, said method comprising the steps of: a) providing a band which consists essentially of, in weight percent, 2.5-4.5% Si, 0.01-0.08% C, 0.009% or less Al, 0.006 to 0.06% S, 0.006-0.14% Se, 0.01-0.10% Mn with a maximum of 0.024% in excess of that needed to combine with S and/or Se, and balance being essentially iron and normally occurring residual elements; b) providing said band having a thickness of: t.sub.o =t.sub.f exp[(K/t.sub.f).sup.0.25 ] where t o is t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (13)
Non-Patent Literature (2)
- "Developments of Grain Oriented Si Steel Sheets with Low Iron Loss", Sadyori et al, Kawasaki Seitetsu Giho, vol. 21, No. 3, pp. 93-98, 1989.
- Developments of Grain Oriented Si Steel Sheets with Low Iron Loss , Sadyori et al, Kawasaki Seitetsu Giho, vol. 21, No. 3, pp. 93 98, 1989.