Process for forming high strength, high modulus polymer fibers
Abstract
Fibers of linear polyethylene or polypropylene are solution spun, cooled, dried in hot air and hot drawn. Drying and hot drawing are carried out by passing a moving filament of the wet polymer through a hot air dryer having an air temperature of at least 55 degrees C., preferably at least 60 degrees C., then heating and hot drawing a moving filament of the dried fiber. Optional steps include wet drawing the fiber prior to drying, and solvent exchange of the original solvent, e.g. decalin, for a more volatile solvent.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 43.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for making a polymer filament having high tensile strength and high modulus, comprising the steps of: (a) spinning a solution of polyethylene or polypropylene having a weight average molecular weight of at least 500,000, and containing from about 0.5 to about 20 weight percent polymer, through an aperture at a temperature above the gelation temperature of the solution and below the boiling point of the solvent, thereby forming a wet spun filament; (b) cooling said wet spun filament without drying to a temperature below the gelation temperature of the polymer solution thereby formin
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 43 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (5)
- B. Kalb and A. J. Pennings, J. Mater. Sci., 15, 2584 (1980).
- B. Kalb and A. J. Pennings, Polymer Bulletin, 1, 871 (1979).
- B. Kalb and A. J. Pennings, Polymer, 21, 3 (1980).
- J. Smook and A. J. Pennings, J. Appl. Polym. Sci., 27, 2209 (1982).
- J. Smook, J. C. Torfs and A. J. Pennings, Makromol. Chem., 182, 3351 (1981).