Thixotropic adhesive gel
Abstract
A water based thixotropic adhesive gel is disclosed which consists essentially of: water; partially hydrolyzed polyvinyl alcohol, or wherein a portion of the polyvinyl alcohol is replaced with polyvinylpyrrolidone; a water-soluble high viscosity thickening agent polymer which is compatible with the polyvinyl alcohol and which imparts thixotropic properties to the gel; a water-soluble plasticizer for the polyvinyl alcohol; and a watersoluble defoamer in proportion of ingredients so that the viscosity of the adhesive will break down when a flexible tube or squeeze bottle dispenser is finger-pressed and have a sufficiently low viscosity to allow for easy extrusion from an orifice having a diameter of about 0.06 to 0.15 inches. When pressure is released, after the desired amount of adhesive has flown out of the dispenser, the adhesive quickly reverts to very close to its original gel state so that it will not run on a vertical surface on porous and semiporous surfaces such as paper. An article of manufacture is also provided whereby the adhesive gel containing the above ingredients is in a flexible dispenser from which the adhesive can be dispensed by finger-pressure.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 28.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A clear, thixotropic adhesive gel consisting essentially of: A. about 70% to 93% of water; B. about 5% to 25% of partially hydrolyzed polyvinyl alcohol; C. about 0.5% to 1.5% of a thickening agent polymer compatible with the polyvinyl alcohol selected from the group consisting of sodium carboxymethylcellulose, sodium alginate, and xanthan gum; D. about 0.5% to 3% of a water-soluble plasticizer for the polyvinyl alcohol; and E. about 0.05% to 0.35% of a water-soluble defoamer.
- Claim 2Depends on #1
The gel of claim 1 wherein: the quantity of thickening agent is sufficient to provide a thixotropic index of from about 1.5 to 4.5 when viscosity of said gel at 20 RPM is divided into the viscosity at 2 RPM of said gel at 25° C. as measured with an RVF Brookfield viscometer using a number 6 spindle.
- Claim 3Depends on #1
The gel of claim 1 wherei
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 28 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (5)
- Handbook of Water Soluble Gums and Resins by R. L. Davidson, 1980, McGraw Hill, pp. 20 18, 20 19, 20 20, 21 15 and 21 16.
- Handbook of Water Soluble Gums and Resins by R. L. Davidson, 1980, McGraw Hill, pp. 20-18, 20-19, 20-20, 21-15 and 21-16.
- Kelco Xanthan Gum, Third Edition of Kelco, a division of Merck & Co.
- Kelzan, Xanthan Gum, (Technical Bulletin DB 15) of Merck & Co.
- Kelzan, Xanthan Gum, (Technical Bulletin DB-15) of Merck & Co.