Patents
US 5,284,290 A#5974285 Most CitedExpiredUnited States (USPTO)Utility

Fusion welding with self-generated filler metal

16Forward Citations (#5974285 Global)
0.5/yrCitation Velocity (#15517902 Global)
1.65Citation PageRank (#19659333 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

NiAl is preheated to a temperature between 1530 DEG C. and 1638 DEG C. causing some of the aluminum to evaporate along the faying surfaces thereby forming a glazed layer of nickel rich self-generated filler metal. The glazed faying surfaces are placed in contact, heated to 1530 DEG C. to 1570 DEG C., and pressed together to form a fusion weld.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 16.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of joining members of a metal alloy containing at least two alloying elements along faying surfaces without the addition of other material, filler metal, or brazing material comprising removing one of said alloying elements from said faying surfaces thereby lowering the solidus and the liquidus temperatures of the alloy at said faying surfaces whereby a glazed layer of the remaining alloying elements is produced, placing said glazed surfaces in contact in a chamber, applying a pressure to said contacting surfaces, and heating said contacting surfaces in said chamber while applyi

  2. Claim 2Depends on #1

    A method of joining members as claimed in claim 1 wherein the members are an intermetallic base metal.

  3. Claim 3Depends on #2

    A method of joining members as claimed in claim 2 wherein the members co

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗