Controlled thermal expansion alloy and article made therefrom
Abstract
A precipitation strengthenable, nickel-cobalt-iron base alloy and articles made therefrom are disclosed. The alloy contains controlled amounts of silicon, nickel, cobalt, iron, chromium, niobium, titanium, and aluminum which are critically balanced to provide a unique combination of high strength, good ductility, and controlled thermal expansion, together with good thermal stability and good oxidation resistance up to about 1200° F. or higher.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 13.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A precipitation strengthenable, nickel-cobalt-iron base alloy consisting essentially of, in weight percent, about Carbon 0.2 max. Manganese 1 max. Silicon 0.1-0.8 Phosphorus 0.015 max. Sulfur 0.010 max. Chromium 2.0-10 Nickel 15-29 Molybdenum 3 max. Cobalt 24-46 Titanium 0.3-2 Aluminum 1 max. Niobium 3-7 Vanadium 0.5 max. Zirconium 0.1 max. Boron 0.02 max. Copper 0.5 max. Tungsten 0.5 max. and the balance is essentially iron, wherein a) ##EQU3## b) ##EQU4## c) the combined amount of niobium, titanium, and aluminum is about 3-7 atomic percent of the alloy;
- Claim 2Depends on #1
An alloy as set forth in claim 1 cont
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (13 of 13 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,066,447 A | Low expansion superalloy | 1978 | 26 |