Patents
US 5,282,946 A#308658 Most CitedExpiredUnited States (USPTO)Utility

Platinum-cobalt alloy sputtering target and method for manufacturing same

88Forward Citations (#308658 Global)
2.8/yrCitation Velocity (#1067640 Global)
14.22Citation PageRank (#591230 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A sputtering target of platinum-cobalt alloy is disclosed which contains 10 to 55% by weight of platinum; 1 to 15% by weight of a first additional element selected from the group consisting of nickel and tantalum; no more than 1.5% by weight of a second additional element selected from the group consisting of boron, titanium, lanthanum, cerium, neodymium, beryllium, calcium, zirconium, and silicon; no more than 20% by weight of chromium; and balance cobalt. A method for manufacturing the sputtering target is also disclosed. In the method, a platinum-cobalt alloy containing specific ingredients in predetermined amounts is first prepared. Then, the platinum-cobalt alloy is subjected to hot plastic working with a thickness reduction of no less than 30%. Subsequently, the alloy thus hot worked is subjected to a cold plastic working with a thickness reduction of no less than 5% at a temperature less than the recrystallization temperature of the alloy.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 88.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A sputtering target of platinum-cobalt alloy consisting essentially of 10 to 55% by weight of platinum; 1 to 15% by weight of a first additional element selected from the group consisting of nickel and tantalum; no more than 1.5% by weight of a second additional element selected from the group consisting of boron, titanium, lanthanum, cerium, neodymium, beryllium, calcium, zirconium, and silicon; no more than 20% by weight of chromium; and the balance cobalt, wherein said alloy has an average grain size of no greater than 20 μm.

  2. Claim 2Depends on #1

    A sputtering target as recited in claim 1, having a magnetic permeability of no larger than 30.

  3. Claim 3Depends on #1

    A sputtering target as recited in claim 1, wherein the chromium constituent has a segregation of no greater than ±0.25% by weight, and the platinum constituent has a segregation of no gr

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Patent Abstracts of Japan, vol. 12, No. 405, Oct. 26, 1988, JP A 63 143258, Masatoshi Fukushima, Sputtering Target .
  • Patent Abstracts of Japan, vol. 12, No. 405, Oct. 26, 1988, JP-A-63-143258, Masatoshi Fukushima, "Sputtering Target".