Patents
US 5,269,984 A#3883280 Most CitedExpiredUnited States (USPTO)Utility

Process of making graphite fiber

21Forward Citations (#3883280 Global)
0.6/yrCitation Velocity (#12263817 Global)
4.26Citation PageRank (#4296650 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A graphite fiber having an elastic modulus E of 340-680 GPa, a microvoid radius of not larger than 20 Å and a crystal size L c (Å) satisfying the following formula: L.sub.c.sup.3 ≦0.918×10.sup.3 E-3×10.sup.5 is valuable for a composite material having an improved compression strength. The graphite fiber is made preferably by oxidizing an acrylonitrile polymer precursor containing 0.05-8 wt. % of comonomer units and having an iodine adsorption amount of not larger than 3 wt. % and an orientation degree of at least 85%, at 200°-300° C. in an oxidative atmosphere under tension to obtain an oxidized fiber having a water adsorption of not larger than 7 wt. % and an orientation degree of at least 78%, followed by carbonization and graphitization of the oxidized fiber under tension.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 21.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for making a graphite fiber, which comprises the steps of: preparing a precursor fiber having an iodine adsorption amount of not larger than 3% by weight and an orientation degree of at least 85%, by spinning a dope of an acrylonitrile copolymer comprised of 92 to 99.95% by weight of acrylonitrile units and 0.05 to 8% by weight of copolymerized monomer units; oxidizing the precursor fiber at a temperature of 200° to 300° C. in an oxidative atmosphere containing at least 15% by volume of oxygen while being kept under tension during at least a portion of the oxidation to obtain an ox

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 21 total)

PatentTitleYearCitations
WO 2009/049174 A1Carbon fibers and films and methods of making same—17
US 8,674,045 B2Carbon-fiber precursor fiber, carbon fiber, and processes for producing these20145
US 2011189077 A1Microporous graphite foam and process for producing same—4
US 2010143713 A1Carbon fiber, process for production of polyacrylonitrile-base precursor fiber for carbon fiber production, and process for production of carbon fiber—10
US 2010003515 A1Polyacrylonitrile polymer, method of producing the same, method of producing precursor fiber used for producing carbon fiber, carbon fiber and method of producing the same—40
US 6,156,287 AMethod for preparing pan-based activated carbon fabrics200014
US 8,822,029 B2Polyacrylonitrile polymer, method of producing the same, method of producing precursor fiber used for producing carbon fiber, carbon fiber and method of producing the same20141
US 6,635,199 B2Process for producing a precursor fiber bundle and a carbon fiber bundle20035
EP 2,075,810 A2Carbon fibers fabric electrode for supercapacitor and method for manufacturing the same—0
US 7,976,945 B2Flame resistant fiber, carbon fiber and production method thereof20110
US 2005281730 A1Microporous graphite foam and process for producing same—14
US 6,294,252 B1Precursor fiber bundle for production of a carbon fiber bundle, a process for producing the precursor fiber bundle, a carbon fiber bundle, and a process for producing the carbon fiber bundle20018
US 8,137,810 B2Carbon fiber, process for production of polyacrylonitrile-base precursor fiber for carbon fiber production, and process for production of carbon fiber20127
US 2011038788 A1Carbon-fiber precursor fiber, carbon fiber, and processes for producing these—21
US 2010086762 A1Solution containing flame-resistant polymer and carbon molding—0