Apparatus for forming shallow electrical junctions
Abstract
Very shallow electrical junctions may be formed in an oxide free surface of a semiconductor by introducing an inert or reducing gas into a vacuum processing chamber, heating the semiconductor to between 750° C. and 1100° C., introducing a dilute solution of a dopant gas into the chamber, and exposing the semiconductor to the gases for about 0.5 to about 100 minutes, preferably between 10 and 30 minutes. A relatively wide range of surface dopant concentrations may be achieved thereby with dopant concentration controlled independent of junction depth. Non-oxide free semiconductor surfaces may be made oxide free by first heating the semiconductor surface in the presence of the reducing gas. This technique provides uniform surface dopant concentrations and is suitable for the formation of junctions in deep trenches and other features having high aspect ratios.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 12.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Apparatus for forming electrical junctions in semiconductor material comprising: means for forming an oxide free region on the surface of a semiconductor material; means for heating the oxide free region to a temperature in the range of about 750° C. to about 1100° C.; means for exposing the oxide free region to a dilute concentration of dopant gas at a pressure over the range from about 10 -1 Torr to atmospheric pressure; and means for controlling the duration of exposure of the heated oxide free to the dopant gas in the range of about 0.5 to about 100 minutes.
- Claim 2Depends on #1
The apparatus of claim 1 wherein the means for controlling the duration of exposure further comprises: means for controlling the depth of the junction.
- Claim 3Depends on #1
The apparatus of claim 1 further comprising: means for controlling the concentration
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,855,258 A | Native oxide reduction for sealing nitride deposition | 1989 | 36 |
| US 5,124,272 A | Method of producing field effect transistor | 1992 | 52 |
Non-Patent Literature (5)
- Barry, et al. "Doped Oxides As Diffusion Sources", Solid State Science, vol. 116, No. 6, Jun., 1969. (pp. 854-860).
- Barry, et al. Doped Oxides As Diffusion Sources , Solid State Science, vol. 116, No. 6, Jun., 1969. (pp. 854 860).
- Fisher, et al. "Diffusion Characteristics and Applications of Doped Silicon Dioxide Layers Deposited From Silane", RCA Review, vol. 29, Dec., 1968. (pp. 533-548).
- Fisher, et al. Diffusion Characteristics and Applications of Doped Silicon Dioxide Layers Deposited From Silane , RCA Review, vol. 29, Dec., 1968. (pp. 533 548).
- Michel, et al. "Anomalous Diffusion of Boron Implanted Into Silicon Along The [100] Direction", Applied Physical Letters, vol. 53, No. 10, Sep. 5, 1988. (pp. 851-853).