Cathode-ray tube with low reflectivity film
Abstract
A cathode-ray tube includes a face plate having a light transmittance of at most 50% and a reflectivity reduction film formed on the external surface of the face plate to reduce reflectivity of an external light. The reflectivity reduction film is a low refraction index layer formed by using a coating liquid obtained by dispersing and mixing magnesium fluoride superfine particles to a base coating of an alcohol solution containing a silicon alkoxide. The low refraction index layer can be laminated by a high refraction index layer formed by using a coating liquid obtained by dispersing and mixing tantalum oxide fine particles to the same base coating as that of the low refraction index layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 34.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A cathode-ray tube comprising: a face plate having a light transmittance of at most 50%, and a reflectivity reduction film formed on a front surface of the face plate, the reflectivity reduction film being a silicia layer having magnesium fluoride supefine particles having an average particle size of at most 100 nm dispersed therein; said reflectivity reduction film being of a predetermined thickness satisfying the following formula 480≦4nd/(2m-1)≦620 wherein d is a thickness of said reflectivity reduction film, n is a refractive index, and m is a positive integer.
- Claim 2Depends on #1
The cathode-ray tube of claim 1, wherein said refraction index n of said reflectivity reduction film is approximately 1.4.
- Claim 3Depends on #2
The cathode-ray tube of claim 2, wherein an average particle size of said magnesium fluoride superfine parti
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗