Method for making mullite whiskers using hydrofluoric acid

1Forward Citations (#56887719 Global)
0.0/yrCitation Velocity (#58721405 Global)
0.80Citation PageRank (#56887719 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for making mullite whiskers includes the steps of: preparing a mullite-intensive sol by mixing an alumina sol with a silica sol at a molar Al 2 O 3 /SiO 2 ratio of 1.37-1.76, gelating said mullite-intensive sol by adding HF thereto at a molar HF/3Al 2 O 3 ·2SiO 2 ratio of 0.01-0.1, drying the gel at a temperature lower than 120° C.; and calcining the dried product in an open system at a temperature up to 1000° C. and in a closed system at a temperature from 1200°-1600° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for making mullite whiskers, which includes the steps of: preparing a mullite-intensive sol by mixing an alumina sol with a silica sol, gelating said mullite-intensive sol by adding hydrofuloric acid thereto, drying the gel obtained at the gelation step; and calcining the dried product obtained at the drying step.

  2. Claim 2Depends on #1

    A method for making mullite whiskers as claimed in claim 1, wherein said alumina and silica sols are mixed together at a molar Al 2 O 3 /SiO 2 ratio in the range of 1.37 to 1.76.

  3. Claim 3Depends on #1

    A method for making mullite whiskers as claimed in claim 1, wherein hydrofluoric acid is added at a molar HF/3Al 2 O 3 ·2SiO 2 ratio in the range of 0.01 to 0.1.