Patents
US 5,228,977 A#4644576 Most CitedExpiredUnited States (USPTO)Utility

Method of producing asphalt having an increased penetration and penetration index

19Forward Citations (#4644576 Global)
0.6/yrCitation Velocity (#13646606 Global)
2.46Citation PageRank (#10433848 Global)
3Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

This invention relates to a method for producing asphalt that has improved low temperature properties. More specifically, the penetration and Penetration Index of an asphalt can be increased if the asphalt is heat soaked in the presence of a dehydrogenation agent at a temperature above the temperature at which oxidation of the asphalt occurs and below the temperature at which coking is initiated. Polyvinyl chloride and a chlorinated wax are preferred dehydrogenation agents.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 19.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing a softer asphalt product with improved low temperature properties from an asphalt feed which comprises measuring the penetration and Penetration Index of the asphalt feed and heat soaking the asphalt feed in the presence of a dehydrogenation agent, wherein from about 0.05 to about 10 wt. % of the hydrogenation agent, based on weight of the asphalt, is present during heat soaking, at a temperature ranging between about 300° and about 400° C., said temperature being sufficient to increase the penetration and Penetration Index over that of the asphalt feed provided that the

  2. Claim 2Depends on #1

    The method of claim 1 wherein the dehydrogenation agent is selected from the group consisting of air, aluminum trichloride, boric acid, boron trifluoride, chlori

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗