Asphalt paving mix and method for making it
Abstract
An asphalt paving mix preferably comprising a mixture of asphalt oil preferably in the range of between about 18 and 22 percent by weight; mineral wool fiber preferably in the range of 17 and 23 percent by weight and having a length of between about 0.5 and 5.0 inches and a shot content of between about 25 and 35 percent by weight and aggregate material preferably in the range of between about 55 and 65 percent by weight and having a particle size not less than 0.060 inch and methods for making the asphalt paving mix.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 12.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
An asphalt paving mix comprising: a mixture having between about 15 and 30 percent by weight of an asphalt oil; between about 10 and 30 percent by weight of a mineral fibrous material and between about 50 and 70 percent by weight of an aggregate filler material; and said mineral fibers having a length of between about 0.5 to 5.0 inches.
- Claim 2Depends on #1
The invention as in claim 1 wherein said mineral fibrous material comprises: mineral wool fibers formed from slag.
- Claim 3Independent Claim
An asphalt paving mix for forming roads and highways comprising: a mixture having between about 18 and 22 percent by weight of an asphalt oil; between about 17 and 23 percent of a mineral fibrous material and between about 55 and 65 percent by weight of an aggregate material; and said mineral fibers having a length of between about 0.5 to 5.0 inches.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗