Method of producing a felted porous polychloroprene latex foam

5Forward Citations (#20787234 Global)
0.1/yrCitation Velocity (#38459207 Global)
1.50Citation PageRank (#22787804 Global)
17Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of felting porous polychloroprene latex foam to obtain desired properties. Such felting renders the finished foam suitable for controlled ink flow required for printing purposes. The felting is accomplished by reducing the volume of the porous polychloroprene latex foam and heating at a temperature of 400° to 460° F. for five to ten minutes.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    In a method of making a rechargeable inking member, the steps comprising: a) producing a first inking layer by placing a layer of open cell polychloroprene latex foam in a press, b) the first inking layer by reducing the volume of the first inking layer and subjecting it to a pressure of 11,000 to 13,000 lb/in 2 , and heating the first inking layer to a temperature of 400°-425° F. for 5 to 10 minutes, c) removing the first inking layer from the press, and d) attaching the first inking layer to a second inking layer.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the step of attaching the first layer to the second layer is by applying a polyamide between the first and second layers and heating at a temperature of 220° to 270° F. for a period of 2 to 4 minutes under a pressure of 4,500 to 5,500 lb/in 2 .