Patents
US 5,213,639 A#169875 Most CitedExpiredUnited States (USPTO)Utility

Damage tolerant aluminum alloy products useful for aircraft applications such as skin

117Forward Citations (#169875 Global)
3.5/yrCitation Velocity (#615287 Global)
23.03Citation PageRank (#263923 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of producing a sheet product and improved products having improved levels of toughness and fatigue crack growth resistance at good strength levels. The method comprises providing an aluminum base alloy containing 4 to 4.5% Cu, 1.2 to 1.5% Mg, 0.4 to 0.6% Mn, 0.12% max. Fe, 0.1% max. Si, the remainder aluminum, incidental elements and impurities and hot rolling the alloy, heating the alloy to above 910 DEG F. and additionally hot rolling it in a range of about 600 DEG to 900 DEG F., solution heat treating, preferably for a time of less than about 15 minutes at a solution heat treating temperature, and rapidly cooling and naturally aging. The invention products have very good combinations of strength together with high fracture toughness or low fatigue crack growth rate, or both, making them well suited for aerospace applications such as fuselage skin. The products preferably include a corrosion protecting cladding of aluminum or aluminum alloy.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 117.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing an aluminum product comprising: (a) providing stock comprising an aluminum alloy consisting essentially of, by weight, about 3.8 to 4.5% copper, about 1.2 to 1.8% magnesium, about 0.3 to 0.9% manganese, the remainder substantially aluminum, incidental elements and impurities; (b) hot working said stock; (c) heating said stock above about 895° F. to less than 975° F.; (d) hot rolling said stock; (e) solution heat treating; (f) cooling.

  2. Claim 2Depends on #1

    The method according to claim 1 wherein said alloy contains one or more elements from the group consisting of 0.02 to 0.4 % Zr, 0.01 to 0.5% V, 0.01 to 0.4% Hf, 0.01 to 0.2% Cr, 0.01 to 1% Ag and 0.01 to 0.5% Sc, percentages being by weight.

  3. Claim 3Depends on #1

    The method according to claim 1 wherein said alloy contains less

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Aluminum Alloy Development for Subsonic and Supersonic Aircraft", M. V. Hyatt, et al., Science and Engineering of Light Metals, published by The Japan Institute of Light Metals, Tokyo, Oct. 1991, pp. 273 to 280.
  • Aluminum Alloy Development for Subsonic and Supersonic Aircraft , M. V. Hyatt, et al., Science and Engineering of Light Metals, published by The Japan Institute of Light Metals, Tokyo, Oct. 1991, pp. 273 to 280.
  • J. E. Hatch: "Aluminium", vol. 1, "Properties and Physical Metallurgy", 1st Edition, 1984, pp. 268-269, 361-365, 372-374, American Society for Metals, Metals Park, Ohio, US.
  • J. E. Hatch: Aluminium , vol. 1, Properties and Physical Metallurgy , 1st Edition, 1984, pp. 268 269, 361 365, 372 374, American Society for Metals, Metals Park, Ohio, US.
  • Metals Handbook, vol. 2, "Properties and Selections: Nonferrous Alloys and Pure Metals", 9th Edition, 1979, pp. 50, 72-75, American Society for Metals, Metals Park, Ohio, US.