Patents
US 5,213,612 A#1528351 Most CitedExpiredUnited States (USPTO)Utility

Method of forming porous bodies of molybdenum or tungsten

38Forward Citations (#1528351 Global)
1.1/yrCitation Velocity (#5401395 Global)
5.62Citation PageRank (#2740924 Global)
2Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for forming a porous body of a metal from the group consisting of molybdenum, molybdenum alloy, tungsten, tungsten alloy, or mixtures thereof comprises foaming a mixture of a sinterable powder of the metal and a foaming agent in a volume ratio of about 0.6 to 3.5:1 respectively, to form a foam having the metal powder dispersed therein. The foam is heated in a reducing atmosphere that promotes interparticle diffusion and bonding, to decompose the foam and sinter the metal powder to form the porous body.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 38.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a porous body of a metal from the group consisting of molybdenum, molybdenum alloys tungsten, tungsten alloys or mixtures thereof comprising: foaming a mixture of a sinterable powder of the metal and a foaming agent in a volume ratio of about 0.6 to 3.5:1 respectively, to form a foam having the metal powder dispersed therein; and heating the foam in a reducing atmosphere that promotes interparticle diffusion and bonding, to decompose the foam and sinter the metal powder to form the porous body.

  2. Claim 2Depends on #1

    A method according to claim 1 wherein the powder has a particle size of about 10 microns or less.

  3. Claim 3Depends on #2

    A method according to claim 2 wherein the heating is at a rate of about 80° C. per minute or less.