Patents
US 5,207,263 A#19293839 Most CitedExpiredUnited States (USPTO)Utility

VLS silicon carbide whisker reinforced metal matrix composites

5Forward Citations (#19293839 Global)
0.1/yrCitation Velocity (#38307011 Global)
2.31Citation PageRank (#11530699 Global)
29Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for preparing vapor-liquid-solid silicon carbide whisker reinforced metal matrix composites by a squeeze casting process employing a primary pressure and then a hydrostatic pressure to form the reinforced composites. The process to make the composites comprises: 1) providing VLS silicon carbide whiskers in a mold cavity; 2) introducing a molten metal into the mold cavity; 3) subjecting the molten metal and VLS silicon carbide whiskers in the cavity to a primary pressure of about 100 psi to about 2000 psi to infiltrate the whiskers with the molten metal; 4) subsequently subjecting the VLS silicon carbide whiskers infiltrated with the molten metal to a hydrostatic pressure of about 10,000 psi to about 25,000 psi to produce a fully dense mass; and 5) solidifying the metal matrix to form a composite.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a whisker reinforced metal matrix composite material comprising: 1) providing VLS silicon carbide whiskers in a mold cavity; 2) introducing a molten metal into the mold cavity; 3) subjecting the molten metal and VLS silicon carbide whiskers in the cavity to a primary pressure of about 100 psi to about 2000 psi to infiltrate the whiskers with the molten metal; 4) subsequently subjecting the VLS silicon carbide whiskers infiltrated with the molten metal to a hydrostatic pressure at about 10,000 psi to about 25,000 psi to produce a fully dense mass; and 5) solidify

  2. Claim 2Depends on #1

    The process of claim 1 wherein the VLS silicon carbide whisker is in the range from about 1% to about 70% by volume in the metal matrix composite material.

  3. Claim 3Depends on #1

    The process of claim 1 wherein

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
US 3,421,862 AHigh strength whisker composite article19697
US 3,529,655 AMethod of making composites of magnesium and silicon carbide whiskers197020
US 3,547,180 AProduction of reinforced composites1970161
US 3,668,748 AProcess for producing whisker-reinforced metal matrix composites by liquid-phase consolidation197231
US 3,695,335 AProcess for making composite materials from refractory fibers and metal19729
US 3,721,732 AMethod of manufacturing filamentary bodies of circular cross-section consisting of silicon carbide single crystals and filamentary bodies obtained by said method197315
DE 1,794,382 A1Versteifung von gegenstaenden aus kunststoff, glas oder metall—2
US 4,013,503 AFilamentary silicon carbide crystals by VLS growth in molten iron197730
US 4,357,986 AMethod of producing a fiber-reinforced composite article19822
US 4,476,916 AMethod of casting metal matrix composite in ceramic shell mold198426
US 4,526,841 AFiber-reinforced metal composite material198511
US 4,534,400 AMethod for making a reinforced article for an internal combustion engine19858
US 4,543,345 ASilicon carbide whisker reinforced ceramic composites and method for making same1985194
US 4,548,774 AMethod for preparing a SiC whisker-reinforced composite material198512
US 4,570,316 AMethod for manufacturing a rotor for a rotary fluid pump198687
US 4,573,519 AMethod for forming metal base composite19866
US 4,606,395 AMethod of producing fiber-reinforced composite material198612
US 4,630,665 ABonding aluminum to refractory materials198672
US 4,633,931 AMethod of producing fiber-reinforced composite body198719
US 4,652,413 AMethod for preparing configured silicon carbide whisker-reinforced alumina ceramic articles198750
US 4,657,065 AComposite materials having a matrix of magnesium or magnesium alloy reinforced with discontinuous silicon carbide particles198770
US 4,662,429 AComposite material having matrix of aluminum or aluminum alloy with dispersed fibrous or particulate reinforcement198781
US 4,674,554 AMetal product fabrication198711
US 4,681,151 AMethod for production of fiber-reinforced metal composite material19879
US 4,749,667 AAlumina - zirconia ceramics reinforced with silicon carbide whiskers and methods of making the same198829

Non-Patent Literature (5)

  • 87 CID 0969, Crack Deflection as a Toughening Mechanism in Silicon Carbide Whisker Reinforced MoSi 2 86 A2C 0537; 86 CID 0589; CA83(18):155876c; CA83(12):106 544; CA83(4):36019r; CA82(6):37409.
  • 87-CID-0969, Crack Deflection as a Toughening Mechanism in Silicon Carbide-Whisker-Reinforced MoSi2 86-A2C-0537; 86-CID-0589; CA83(18):155876c; CA83(12):106 544; CA83(4):36019r; CA82(6):37409.
  • B. R. Henriksen: The microstructure of squeeze Cast SiC w reinforced Al4Cu base alloy with Mg & Ni additions.
  • B. R. Henriksen: The microstructure of squeeze-Cast SiCw -reinforced Al4Cu base alloy with Mg & Ni additions.
  • Composites, vol. 21, No. 4, Jul. 1990, Haywards Health GB, pp. 333 338.