Abstract

A-type fibers having a fiber thickness of less than 1 denier is produced by the steps of: obtaining undrawn fibers by melt-spinning a co-polyester having an intrinsic viscosity of from 0.35 to 0.50, and having repeating units composed mainly of ethylneneterephthalate that contains from 0.5 mol % to 7.0 mol % of 5-sodiumsulfoisophthalic acid and from 0.5 mol % to 10 mol % of isophthalic acid; and flow-drawing the undrawn yarn at a draw ratio of more than 5 times. The A-type polyester fibers are further neck-drawn at a draw ratio of more than 1.05 times to be B-type fibers, and the B-type fibers are subjected to a restricted contraction treatment to be C-type fibers. Staple fibers having a length of less than 15 mm obtained from at least one of the A, B and C-type fibers are blended in a material for the production of a wet type non-woven fabric at a ratio of more than 10 weight %, if necessary, together with other fibers such as a regular type polyester fiber, wood pulp or a glass fiber. The resultant non-woven fabric has a soft hand and a uniform appearance as well as improved mechanical properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 17.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing ultra-fine polyester fibers, consisting essentially of: obtaining undrawn fibers by melt-spinning a co-polyester having an intrinsic viscosity of from 0.35 to 0.50, and having repeating units composed mainly of ethylene-terephthalate that contains from 0.5 mol % to 7.0 mol % of 5-sodium-sulfoisophthalic acid and from 0.5 mol % to 10 mol % of isophthalic acid; and flow-drawing the undrawn fibers at a draw ratio of more than 5 times.

  2. Claim 2Depends on #1

    A method as defined in claim 1, wherein the polyester fibers are further neck-drawn at a draw ratio of more than 1.05 times after the flow-drawing.

  3. Claim 3Depends on #1

    A method as defined in claim 1, wherein the polyester fibers are further neck-drawn at a draw ratio of more than 1.05 times after the flow-drawing, and then are subjected to a restricted contraction treatment in which the

Technical Overview & Description