Patents
US 5,202,153 A#3064155 Most CitedExpiredUnited States (USPTO)Utility

Method for making thick film/solder joints

25Forward Citations (#3064155 Global)
0.8/yrCitation Velocity (#9783373 Global)
3.30Citation PageRank (#6505957 Global)
1Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for making a thick film/solder joint comprising the sequential steps of: (1) applying a layer of first thick film conductor paste to an electrically non-conductive substrate in a pattern which has preselected solder pad areas and firing the layer; (2) applying over the first thick film layer only within the solder pad area a layer of a second thick film conductor paste having a low frit content and firing the layer; and (3) forming the solder joint by applying to the fired second thick film layer a layer of soft solder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 25.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for making thick film/solder joints having a preselected area comprising the sequential steps of (1) applying to an electrically-non-conductive substrate a patterned layer having a preselected solder pad area of a first thick film conductive composition comprising finely divided particles of (a) 85.0-98.5% wt. of a pure unalloyed ductile conductive metal or low alloy thereof having a particle size of 0.5-5 microns, (b) 1-10% wt. inorganic binder; and (c) 0.5 to 5.0% wt. spinel-forming metal oxide, all of (a), (b) and (c) being dispersed in organic medium; (2) firing the first thick

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (1)

Non-Patent Literature (1)

  • U.S. Ser. No. 07/508,769, filed Apr. 12, 1990, by Nebe et al.