High-carbon low-nickel heat-resistant alloys
Abstract
Air-meltable, castable, machinable, weldable heat-resistant alloys that are very resistant to hot gas corrosion and that exhibit high creep rupture strengths. The alloys are, by weight, about 7.5 to aboout 18% nickel, about 23.5 to about 35% chromium, about 0.85 to about 1.4% carbon, about 0.2 to about 1.8% molybdenum, about 0.2 to about 1.6% tungsten, about 0.1 to about 1.6% columbium (niobium), about 0.2 to about 4% manganese, about 0.2 to about 2.5% silicon, up to about 1.5% cobalt, up to about 0.6% titanium, up to about 0.4% zirconium, up to about 0.4% rare earth elements, up to about 0.1% boron, up to about 0.7% nitrogen, and the balance essentially iron plus the usual minor impurities.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 28.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A nickel-chromium-iron alloy consisting essentially of about: ______________________________________ Nickel 7.5-18% by weight Chromium 23.5-35 Carbon 0.85-1.4 Molybdenum 0.2-1.8 Tungsten 0.2-1.6 Columbium 0.1-1.6 Manganese 0.2-4 Silicon 0.2-2.5 Cobalt up to about 1.5 Titanium up to about 0.6
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗