Abstract
A metallic reinforced shim is attached to the dovetail of turbine or compressor blades. The shim reduces frictionally induced wear damage to the rotor. In one form, a single ply shim reinforced with a metallic doubler has an anti-fretting layer deposited on the shim face contacting the dovetail slot pressure face, and a doubler layer fastened to the anti-fretting layer in the non-contacting regions to prevent slippage of the shim on the blade. In another form, a multi-layer shim has two layers interposed between the blade dovetail and the disk dovetail slot, with the layers treated so that they do not readily slip relative to the titanium pieces, but do slip relative to each other. The shim is also reinforced with a metallic doubler. Fretting is confined to the consumable shim, and therefore the disk dovetail slot and the mating blade dovetails are not subject to surface degradation with corresponding reduction in fatigue capability.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 114.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An assembly for a turbine engine, comprising: a titanium rotor having a dovetail slot in a rotor circumference thereof, the dovetail slot including at least a pair of sidewalls diverging in a direction from the circumference toward an inward portion of the rotor, and terminating at a bottom; a titanium blade having a dovetail sized to fit into the dovetail slot and contact the rotor along a pair of contacting regions on the inwardly diverging sidewalls of the dovetail slot, one contacting region being located on each side of the dovetail slot, there remaining a non-contacting region between
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗