Patents
US 5,154,987 A#16263046 Most CitedExpiredUnited States (USPTO)Utility

Highly conductive electrolyte composites containing glass and ceramic, and method of manufacture

6Forward Citations (#16263046 Global)
0.2/yrCitation Velocity (#35000100 Global)
4.61Citation PageRank (#3778510 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An electrolyte composite is manufactured by pressurizing a mixture of sodium ion conductive glass and an ionically conductive compound at between 12,000 and 24,000 pounds per square inch to produce a pellet. The resulting pellet is then sintered at relatively lower temperatures (800° C.-1200° C.), for example 1000° C., than are typically required (1400° C.) when fabricating single constituent ceramic electrolytes. The resultant composite is 100 percent conductive at 250° C. with conductivity values of 2.5 to 4×10 -2 (ohm-cm) -1 . The matrix exhibits chemical stability against sodium for 100 hours at 250° to 300° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating electrolyte composites comprising: mixing sodium-ion conductive glass with an ionically conductive compound in a 50:50 weight percent ratio to produce a mixture where the sodium ion conductive glass wets the ionically conductive compound; shaping the mixture by pressing between 12,000 pounds per square inch and 24,000 pounds per square inch; and heating the mixture at a temperature less than 1400° C.

  2. Claim 2Depends on #1

    A method as recited in claim 1 wherein the conductive compound is selected from the group consisting of β-alumina, β'-alumina, β"-alumina, sodium yttrium oxide, NASICON ceramic and combinations thereof.

  3. Claim 3Depends on #1

    A method as recited in claim 1 wherein the conductive compound is β"-alumina.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗