Patents
US 5,153,264 A#27010258 Most CitedExpiredUnited States (USPTO)Utility

Poly(arylene thioether) block copolymer and production process thereof

4Forward Citations (#27010258 Global)
0.1/yrCitation Velocity (#43146343 Global)
1.12Citation PageRank (#35533533 Global)
33Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed herein are a poly(arylene thioether) block copolymer alternately comprising (A) at least one poly(arylene thioether-ketone) block having predominant recurring units of the formula <IMAGE> wherein the -CO- and -S- are in the para position to each other and (B) at least one poly(arylene thioether) block having predominant recurring units of the formula <IMAGE> (a) the ratio of the total amount of the poly(arylene thioether) block (B) to the total amount of the poly(arylene thioether-ketone) block (A) being within a range of 0.05-5 by weight, (b) the average polymerization degree of the poly(arylene thioether) block (B) being at least 10, and (c) said block copolymer having a melt viscosity of 2-100,000 poises as measured at 350 DEG C. and a shear rate of 1,200/sec as well as a production process the poly(arylene thioether) block copolymer. The invention also provides a stabilized poly(arylene thioether) block copolymer containing a basic compound either alone or in combination with an antioxidant.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the production of a poly(arylene thioether) block copolymer comprising (A) at least one poly(arylene thioether-ketone) block and (B) at least one poly(arylene thioether) block, which comprises at least the following two steps: i) heating in the presence of water an organic amide solvent containing a dihalogenated aromatic compound, which consists principally of a dihalobenzene, and an alkali metal sulfide, whereby a reaction mixture containing a poly(arylene thioether) prepolymer having predominant recurring units of the formula ##STR27## and reactive terminal groups is formed,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (33)

PatentTitleYearCitations
US 3,966,168 APressure responsive valve19765
US 4,486,578 AStabilized polyphenylene sulfide and method for producing same198412
JP S6058435 AMolded polysulfide ketone article—34
JP S60104126 AAromatic polythioether ketone and its preparation—34
DE 3,405,523 A1Verfahren zur herstellung von polyarylensulfidketonen und ihre verwendung zur herstellung von faserverbundmaterialien—35
US 4,588,789 AMethod for the crystallization of poly(arylene sulfide)198621
JP S61221229 AProduction of aromatic poly(thio)ether ketone—26
US 4,690,972 AMethod of producing poly(arylene sulfide) compositions and articles made therefrom198775
US 4,698,415 AMethod for the preparation of polyarylene sulfide with aqueous polyethylene glycol mixture198728
US 4,716,212 APreparation of a high molecular weight poly(arylene sulfide ketone)198743
US RE32595 EProcess for making a laminated bearing utilizing plastics alloy compositions198818
US 4,745,167 APolyarylene sulfide preparation in titanium reaction vessel with two distinct temperature ranges198847
US 4,785,057 APara-phenylene sulfide block copolymer, process for the production of the same198830
US 4,826,906 APoly(arylene thioether-ketone) compositions improved in both melt stability and crystallinity198920
US 4,873,283 AMolded or formed poly(arylene thioether-ketone) articles198912
US 4,886,871 AMelt-stable poly(arylene thioetherketone) and production process thereof198913
US 4,895,924 APoly(arylene thioether-ketone) fibers and production process thereof199010
US 4,895,925 AMelt-stable poly(arylene thioether-ketone) and production process thereof199011
US 4,895,893 AHeat-resistant resin compositions, and heat-resistant molded or formed articles and production process thereof19909
US 4,895,892 AMelt-stable poly(arylene thioether-ketone) compositions199029
US 4,895,921 AWater soluble or dispersible blocked polyisocyanates and a process for their preparation and use199015
US 4,895,691 APoly(arylene thioether-ketone) fibers and production process thereof19904
US 4,897,238 AStretched poly(arylene thioether-ketone) films and production process thereof199017
JP H02182760 APolyphenylenesulfide resin composition—3
US 4,960,555 APoly (arylene thioether) block copolymer fibers and production process thereof199012

Non-Patent Literature (5)

  • A. B. lPort et al., Polymer Degradation and Stability, Feb. 1980 pp. 1 22.
  • A. B. lPort et al., Polymer Degradation and Stability, Feb. 1980 pp. 1-22.
  • Indian J. Chem., vol. 21A, May 1982, pp. 501 502.
  • Indian J. Chem., vol. 21A, May 1982, pp. 501-502.
  • Indian Journal of Pure and Applied Physics, vol. 22, Apr. 1984, pp. 247 248.