Process for preparing a rubber composition having two different molecular weights
Abstract
A rubber composition comprising 100 parts by weight of a rubber component which comprises at least 30% by weight of an emulsion polymerization rubber which is a conjugated diene polymer rubber or conjugated dienestyrene copolymer rubber obtained by emulsion polymerization, has a bound styrene content of 0-65% by weight, contains 20-35% by weight of a component having a molecular weight of not more than 150,000 as measured by a gel permeation chromatography and has a Mooney viscosity, ML 1+4 (100° C.), of 60-160 and a Mooney viscosity difference (ΔMV) of -20 to +5 as defined by the following equation: ΔMV=ML.sub.1+4 (100° C.)-ML.sub.1+15 (100° C.) and 45-200 parts by weight of carbon black. Said rubber composition is excellent in abrasion resistance, breaking strength and high histeresis property in uses in which carbon black or oil is blended at a high-filling rate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 12.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for preparing a rubber composition comprising: i) emulsion polymerizing a conjugated diene or copolymerizing a conjugated diene and styrene wherein the polymerization is initiated sequentially in the presence of alternating quantities of molecular weight regulator to sequentially produce a high molecular weight rubber compound followed by a low molecular weight compound, or visa versa, a low molecular weight rubber compound followed by a high molecular weight rubber compound; wherein the bound styrene content of the rubber obtained by emulsion polymerization is 0-65%, the content o
Technical Overview & Description