A process for preparing a polyester having an inherent viscosity of at least 0.5 comprising (A) preparing an admixture of a molten polyester having an inherent viscosity of less than 0.5, a titanium alkoxide and a 13X zeolite, and (B) subjecting the admixture to a time and temperature sufficient to increase the inherent viscosity of the polyester to at least 0.5.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a polyester having an inherent viscosity of at least 0.5 comprising (A) preparing an admixture of a molten polyester having an inherent viscosity of less than 0.5, a titanium alkoxide and a 13X zeolite, and (B) subjecting the admixture to a time and temperature sufficient to increase the inherent viscosity of the polyester to at least 0.5.

  2. Claim 2Depends on #1

    The process of claim 1 wherein the polyester is derived from terephthalic acid and a diol selected from the group consisting of ethylene glycol, 1,4-butane diol and 1,4-cyclohexanedimethanol.

  3. Claim 3Depends on #1

    The process of claim 1 wherein the amount of zeolite in is the range of 0.5 to 25 weight percent, based on the weight of the polyester.