Abstract
The invention relates to a process making it possible when a refining catalyst is subject preferably in situ to the conventional activation reaction in the presence of hydrogen (generally at above 100° C.) to carry out, as a result of the in situ presence of hydrogen, the sulphurization at the required stoichiometric or non-stoichiometric level of the active metal or metals in the composition of the catalyst. In the absence of hydrogen, the process consists of incorporating into the porosity of the new or regenerated catalyst at least one sulphurizing agent of general formula: R--S(n)--R' in which n is an integer from 3 to 20 and R represents an organic radical. The invention is characterized in that a critical elementary sulphur quantity is added to the sulphurizing agent. This addition makes it possible to adjust the sulphur content of the presulphurized catalyst to values equal to or higher than stoichiometry, to increase the fixed sulphur quantity after activation under hydrogen and to reduce the exothermy phenomena observed during activation.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 17.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a process for the presulphurization treatment of an active metal on an oxide support catalyst which is conducted in the absence of hydrogen employing a sulphurizing agent comprising a solvent solution of a polysulfide of the formula: R--S(n)--R' in which n is an integer from 3 to 20 and R and R', which can be same or different, each represent an organic radical containing 1 to 150 carbon atoms per molecule selected from the group consisting of alkyl radicals, aryl radicals, alkylaryl radicals and arylalkyl radicals and R' can also represent a hydrogen atom, the improvement
- Claim 2Depends on #1
A process according to claim 1, wherein the catalyst is treated ex situ at between 0° and 50° C.
- Claim 3Depends on #1
Process according to claim 1, wherein the presulphurization tre
Technical Overview & Description