The present invention relates to a process for producing a biaxially oriented polyester film. The process is carried out using the following steps: (a) stretching an amorphous film substantially comprising polyethylene terephthalate 1.2 to 4.0 times in the machine direction by single-stage or multi-stage process to obtain a film having an index of birefringence of 1x10-3 to 2.5x10-2; (b) stretching the thus obtained film 1.1 to 3.5 times in the machine direction by single-stage or multi-stage process of 3.0x10-2 to 8.0x10-2 without cooling the film to the glass transition temperature thereof or below; (c) cooling the thus obtained film to the glass transition temperature thereof or below; (d) heating the thus obtained film to the glass transition temperature or higher and stretching the film in the machine direction by a single-stage or multi-stage process at a stretching ratio which brings the overall stretching ratio of 4.0 to 9.0 times; and (e) stretching the thus obtained film at least 3.2 times in the transverse direction. According to the method of the present invention, a biaxially oriented polyester film which is excellent in thickness uniformity and flat and slippery prope

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 20.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a biaxially oriented polyester film, which comprises the sequential steps of, (a) stretching an amorphous film substantially comprising polyethylene terephthalate 1.2 to 4.0 times in the machine direction in one or more stages to obtain a film having an index of birefringence of 1×10 -3 to 2.5×10 -2 , (b) stretching the thus obtained film 1.1 to 3.5 times in the machine direction in one or more stages while keeping the film at a temperature above the glass transition temperature thereof to obtain a film having an index of birefringence of 3.0×10 -2 to 8.0×10 -2 ,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 20 total)

Non-Patent Literature (5)

  • Abstract of Japanese Reference (Kokai) 54 8,672 (Jan. 1979).
  • Abstract of Japanese Reference (Kokai) 54-8,672 (Jan. 1979).
  • Abstract of Japanese Reference (Kokai) 58 118,220 (Jul. 1983).
  • Abstract of Japanese Reference (Kokai) 58-118,220 (Jul. 1983).
  • Database WPI, No. 78 12792A (07) Derwent Abstract.