Ductility microalloyed NiAl intermetallic compounds
Abstract
A NiAl nickel aluminide alloyed with yttrium, optionally gallium, and an element selected from the group consisting of chromium, molybdenum and combinations thereof, having improved room temperature ductility and plastic strain. NiAl nickel aluminide intermetallics alloyed with no more than about 5 atomic percent of additional elements have significantly improved room temperature ductility over conventional unalloyed beta phase nickel aluminides or beta phase nickel aluminides alloyed with higher percentages of additional elements. The NiAl nickel aluminide comprises, in atomic percent, at least 50% nickel, about 0.01% to about 0.25% yttrium, about 0 to about 0.15% gallium, about 0.05% to about 4% of an element selected from the group consisting of chromium, molybdenum and combinations thereof, and balance from about 40% to about 49.85% aluminum and trace impurities.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 28.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A NiAl intermetallic alloy comprising, in atomic percent, at least about 50% nickel, about 0.01% to about 0.25% yttrium, about 0 to about 0.15% gallium and about 0.05% to about 4% of an element selected from the group consisting of chromium and molybdenum and combinations of chromium and molybdenum, and balance from about 40% to about 49.85% aluminum and trace impurities.
- Claim 2Depends on #1
A NiAl intermetallic article having the composition of claim 1.
- Claim 3Depends on #2
The article of claim 2 wherein the article is a turbine disk for a turbine engine.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 28 total)
References Cited — Backward Prior Art (21)
Non-Patent Literature (5)
- "Mechanical Properties of Intermetallics at High Temperatures", (ASM/TMS Materials Week, Indianapolis 1989); G. Sauthoff; ASM/TMS Symposium on Intermetallics (1989).
- Deformation Behavior of NiAl Based Alloys Containing Iron, Cobalt and Hafnium, D. Pank, M. Nathal, D. Koss, 133 Mat. Res. Soc. Symp. Proc. 561 (1989).
- Deformation Behavior of NiAl--Based Alloys Containing Iron, Cobalt and Hafnium, D. Pank, M. Nathal, D. Koss, 133 Mat. Res. Soc. Symp. Proc. 561 (1989).
- Dislocation Creep in the Ordered Intermetallic (Fe, Ni) Al Phase, M. Rudy and G. Sauthoff, 81 Materials Science and Engineering 525 (1986).
- Improving the Low Temperature Ductility of NiAl, S. Guha, P. Munroe, I. Baker, 133 Mat. Res. Soc. Symp. Proc. 633 (1989).