High density hexagonal boron nitride prepared by hot isostatic pressing in refractory metal containers
Abstract
Boron nitride powder with less than or equal to the oxygen content of starting powder (down to 0.5% or less) is hot isostatically pressed in a refractory metal container to produce hexagonal boron nitride with a bulk density greater than 2.0 g/cc. The refractory metal container is formed of tantalum, niobium, tungsten, molybdenum or alloys thereof in the form of a canister or alternatively plasma sprayed or chemical vapor deposited onto a powder compact. Hot isostatic pressing at 1800° C. and 30 KSI (206.8 MPa) argon pressure for four hours produces a bulk density of 2.21 g/cc. Complex shapes can be made.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 28.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of densifying hexagonal boron nitride comprising: placing boron nitride powder in a refractory metal container consisting essentially of tantalum, niobium, tungsten, molybdenum or alloys thereof; hot isostatically pressing the refractory container filled with boron nitride powder at about 1800 C. and at about 30 KSI (206.8 MPa) to form boron nitride with a bulk density greater than 2.0 g/cc and an isotropically uniform microstructure.
- Claim 2Depends on #1
The method of claim 1 further comprising: forming the refractory metal container with a wall thickness of about 1.6 mm.
- Claim 3Depends on #1
The method of claim 1 wherein the container is a refractory metal canister.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗