Abstract

An aluminum casting alloy consisting of, by weight, of 7.0-13.0% copper, 0.4-1.2% manganese, 0.21-0.40% vanadium, 0.31-0.70% zirconium; impurities limited to: less than to 0.6% Si, less than 0.8% Fe, less than 0.2% zinc, less than 0.1% Mn, less than 0.2% Ni, and the remainder being essentially aluminum. There is an absence of titanium, cobalt, molybdenum, tungsten, chromium, boron, tantalum, and niobium. The alloy has, at room temperature, a UTS of about 61 ksi, a YS of about 49 ksi, a tensile elongation of about 6%, and tensile modulus elasticity of about 11.5 MSi, a compressive yield strength of about 53 ksi, a compressive modulus of elasticity of about 18 MSi; high temperature physical properties at 500° F., after 1000 hours exposure to 500° F., comprise a tensile strength of 33 ksi or greater, a tensile yield strength of 23 ksi or greater, a tensile elongation of about 9%, and tensile modulus of elasticity of 10 msi. The alloy is fabricated by a) squeeze casting an aluminum alloy melt of such character; (b) extracting the solidified casting from the die and heat treating the casting to dissolve all alloying elements (i.e., 995°-1018° F. for 7-20 hours); and (c) aging the soluti

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 22.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A piston having a plurality of annular piston ring grooves and a crown, the ring groove most adjacent the piston crown being spaced therefrom by a wall having a thickness of 0.02-0.05 inches, said wall retaining its strength characteristics at combustion chamber temperatures when deployed in an internal combustion engine with little or no dimensional change, said piston being formed of an aluminum alloy consisting of, by weight, the following: 7.0-13.0% copper, 0.4-1.2% manganese, 0.21-0.40% vanadium, 0.31-0.70% zirconium, in which the levels of V and Zr raise the bulk lower solidification tem

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗