Abstract
The invention relates to a process for the preparation of polyester and alkyd resins from bifunctional and/or polyfunctional carboxylic acids and/or derivatives thereof and from bifunctional and/or polyfunctional alcohols. The reaction is carried out in stirred kettle reactors which are operated discontinuously and equipped with rectifying columns. During the entire reaction an entraining agent is introduced into the reaction mixture below surface level, with thorough distribution, by means of a delivery device in order to improve the transport of the products of the condensation reaction. In addition, the condensation reaction is carried out under an absolute pressure of 1.5 to 10 bar at least until the maximum reaction rate has been reached. The pressure is then reduced to atmospheric pressue at a gradient of -0.05 bar/hour to -5 bar/hour in a second reaction phase. The reaction is continued under normal pressure until the product exhibits the desired properties. The reaction temperature is between 180 and 320° C. The process times, in particular, are shortened as a result of this process, and the process products, which are exposed to heat for a correspondingly shorter time, are
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Process for the preparation of polyester and alkyd resins from bifunctional and/or polyfunctional carboxylic acids and/or carboxylic anhydrides and/or carboxylic acid esters and from bifunctional and/or polyfunctional alcohols, in which the reaction is carried out with the application of pressure in stirred kettle reactors which are operated discontinuously and equipped with rectifying columns, wherein A) the reaction temperature is between 180° and 320° C. B) during the entire process an entraining agent is introduced into the reaction mixture below surface level by means of a delivery devi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 5,760,161 A | Process for making unsaturated, thermosetting, brominated phthalic anhydride/polyol polyester resins | 1998 | 2 |
References Cited — Backward Prior Art (2)
Non-Patent Literature (5)
- Chem. Abstracts, vol. 81, No. 6, 12; Aug. 1974 (Columbus, Ohio) (Kanelafuchi Spinning Co. Ltd Abstract 26194).
- Chem. Abstracts, vol. 81, No. 6, 12; Aug. 1974 (Columbus, Ohio) (Kanelafuchi Spinning Co. Ltd-Abstract #26194).
- Chem. Abstracts, vol.98, No. 20, 16 May 1982 (Columbus, Ohio, U.S.), Abstract #161746m YCS, A, 203350 (Leser F. et al); Oct. 15, 1982.
- Chem. Abstracts, vol.98, No. 20, 16 May 1982 (Columbus, Ohio, U.S.), Abstract 161746 m YCS, A, 203350 (Leser F. et al); Oct. 15, 1982.
- International Polymer Science & Term (Rapra), vol. 12, No. 4 1985 (Shawbury, Shrewbury, GB) F. Leser: "Equipment".