Patents
US 5,114,640 A#7270034 Most CitedExpiredUnited States (USPTO)Utility

Time-efficient process for making expanded polymeric products with multipass expansion of polystyrene bead

13Forward Citations (#7270034 Global)
0.4/yrCitation Velocity (#20902657 Global)
4.06Citation PageRank (#4657769 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for making low density (0.8-1.1 lb./cu.ft.) expanded polymeric products uses blowing agent in an amount of any from 2 to 4.4 weight percent and aging periods of from 1 to 80 hours after each expansion step. The process uses 2 to 5 expansion steps and a polymer having a particular polydispersity, weight average molecular weight and M z :M n , this polymer having a greater expandability than conventional polymers. The process requires only about half of the amount of blowing currently being used in commercially viable processes for making expanded polystyrene products. The process can be used with or without a molding step.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for making an expanded polymeric molded product, the process comprising the steps of: A. preexpanding unexpanded beads in from 2 to 4 preexpansion steps, the beads being comprised of: i. a blowing agent which is at least one member selected from the group consisting of: pentane, cyclopentane, methylcyclopentane, neopentane, isopentane, pentane petroleum distillate fractions), propane, butane, isobutane, hexane, isomers of hexane, methylcyclohexane, cyclohexane, heptane, propylene, 1-butylene, 2-butylene, isobutylene, mixtures of one or more aliphatic hydrocarbons having a molecular w

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗